| Auteur | Rechercher : Jones, S. J.; Rechercher : Spencer, P. A.; Rechercher : Masterson, D. M.; Rechercher : Gagnon, R. E. |
|---|
| Commanditaire | Rechercher : INSROP; Rechercher : National Research Council Canada; Rechercher : CANMAR; Rechercher : NEB |
|---|
| Format | Texte, Article |
|---|
| Conférence | INSROP Symposium, Tokyo, Japan, 1995 |
|---|
| Sujet | ice; flat jack; ice strength |
|---|
| Résumé | Results are presented of flaking tests using flat jacks to measure the large scale strength of ice. The results showed (i) gas-filled flat jacks worked well provided certain safety precautions were taken (ii) the use of a stiff aluminum plate in conjunction with the compliant flat jack reduced the measured pressures somewhat, but they were still around 5.5 Mpa, and (iii) two tests on pre-damaged ice gave significantly reduced pressures of about 1.5 MPa. |
|---|
| Date de publication | 1995 |
|---|
| Langue | anglais |
|---|
| Identificateur | IR-1995-22 |
|---|
| Numéro du CNRC | NRC-IOT-5866 |
|---|
| Numéro NPARC | 8895151 |
|---|
| Exporter la notice | Exporter en format RIS |
|---|
| Signaler une correction | Signaler une correction (s'ouvre dans un nouvel onglet) |
|---|
| Identificateur de l’enregistrement | 6de99c4a-0f7f-4702-8185-600d6922ff6b |
|---|
| Enregistrement créé | 2009-04-22 |
|---|
| Enregistrement modifié | 2025-12-18 |
|---|